Call Us: +86 15954941919 interested in Contact Us? Mail us now
English

Product Description
Alloy seamless steel pipe contains a lot of Cr, and its high temperature resistance, low temperature resistance, and corrosion resistance are not comparable to other seamless steel pipes. Therefore, alloy pipes are widely used in petroleum, chemical, electric power, boilers and other industries.
42CrMo steel belongs to alloy structural steel in terms of material classification. It has good mechanical properties and machinability. It is widely used. There are mainly two types of materials: plate and round bar. Its comprehensive performance is better than 40cr and has been recognized by the industry.
Russia ГOCT 38XM,
American AISI 4140/4142,
UK BS 708M40/708A42/709M40,
French NF 40CD4/42CD4,
German DIN 41CrMo4/42CrMo4,
Japan JIS SCM4,
International ISO 683/1 3
42CrMo steel is an ultra-high strength steel with high strength and toughness, good hardenability, no obvious temper brittleness, high fatigue limit and multiple impact resistance after quenching and tempering treatment, and good low temperature impact toughness. 42CrMo steel is suitable for the manufacture of large and medium-sized plastic molds that require certain strength and toughness .
Carbon C: 0.38~0.45%
Silicon Si: 0.17~0.37%
Manganese Mn: 0.50~0.80%
Sulfur S: allowable residual content ≤ 0.035%
Phosphorus P: allowable residual content ≤ 0.035%
Chromium Cr: 0.90~1.20%
Nickel Ni: allowable residual content ≤ 0.30%
Copper Cu: allowable residual content ≤ 0.30%
42CrMo steel
Molybdenum: 0.15 to 0.25%
Hardness: Annealed, 147~241HB, 42CrMo
42CrMo mechanical properties:
Tensile strength σb (MPa): ≥1080(110)
Yield strength σs (MPa): ≥930(95)
Elongation δ5 (%): ≥12
Area shrinkage ψ (%): ≥45
Impact energy Akv (J): ≥63
Impact toughness αkv (J/cm2): ≥78(8)
Hardness: ≤217HB
In order to increase the life of the mold to more than 800,000 mold times, the pre-hardened steel can be hardened by quenching and low-temperature tempering. When quenching, preheat at 500-600℃ for 2-4 hours, then keep at 850-880℃ for a certain period of time (at least 2 hours), put it in oil and cool it to 50-100℃, and let it cool in oil and air. After quenching, the hardness can reach 50 -52HRC, in order to prevent cracking, it should be tempered at a low temperature of 200 °C immediately. After tempering, the hardness can be maintained above 48HRC.
Neutral salt bath vanadium infiltration treatment process of 42CrMo steel, carbide infiltration layer can be obtained by neutral salt bath vanadium infiltration treatment of 42CrMo steel.
1. Carbon vanadium compound, the infiltration layer has uniform structure, good continuity and compactness, uniform thickness, compact structure, high microhardness and high wear resistance, surface hardness, wear resistance and resistance Adhesion and other properties are greatly improved.
2. The solubility of VC in austenite is higher than its solubility in ferrite. With the decrease of temperature, VC is precipitated from ferrite, which strengthens the alloy and refines the grains, and the compound layer shows higher hardness. . 42CrMo steel is a high-carbon and high-chromium ledeburite steel with a high carbide content, accounting for about 20%, and is often unevenly distributed in a band or network, with serious segregation. Conventional heat treatment is difficult to change the status of carbide segregation. It seriously affects the mechanical properties of the steel and the service life of the mold. The shape and size of carbides also have a great influence on the properties of steel. In particular, the large and sharp-angled carbides have a relatively large splitting effect on the steel matrix, which often becomes the source of fatigue fracture. Change the forging to fully crush the eutectic carbide to make it small and evenly distributed, and the fiber structure is distributed around the cavity or non-directionally, thereby improving the transverse mechanical properties of the steel.
During forging, the billet is upsetting and drawn from different directions for many times, and the "two light and one heavy" method is used for forging, that is, the billet should be struck lightly at the beginning of forging to prevent breakage, and it can be hit hard at the intermediate temperature of 980-1020 ℃. In order to ensure that the carbides are broken, the 42CrMo steel has not been forged, and is treated with solid solution double refinement, that is, secondary preheating at about 500 ℃ and 800 ℃, solution treatment at 1 100 ~ 1 150 ℃, quenching into hot oil or isothermal quenching , Tempering at a high temperature of 750 ℃, heating oil at 960 ℃ after machining, and then performing final heat treatment, which can also refine the carbides, round the edges and corners, and refine the grains.
Recommended tempering specification for 42CrMo steel
Program | Quenching temperature/℃ | tempered | |||
use | Heating temperature/℃ | medium | Hardness HB | ||
Ⅰ II Ⅲ | 1020~1040 | stress relief Relieve stress, reduce hardness Relieve stress, reduce hardness | 150~170 200~275 400~425 | oil or nitrate — — | 61~63 57~59 55~57 |
Ⅳ Ⅴ VI | 1115~1130 | stress relief and secondary hardening stress relief and secondary hardening stress relief and secondary hardening | 510~520℃ multiple tempering -78℃ cold treatment Add 510~520℃ for one tempering -78℃ cold treatment plus one tempering at 510~520℃, and then -78℃ cold treatment | — — — | 60~61 60~61 61~6 |
Program | First preheat/℃ | Second preheat/℃ | Quenching temperature/℃ | cool down | cooling in medium | Medium temperature/℃ | medium | hardness (HRC) |
Ⅰ II Ⅲ Ⅳ Ⅴ | 550~660 | 840~860 | 950~1000 1020~1040 1020~1040 1115~1130 1115~1130 | Oil Oil Molten Nitrate Oil Molten Nitrate | 20~60 20~60 400~550 20~60 400~450 | to room temperature to oil temperature 5~10min to oil temperature 5~10min | air cooling air cooling air cooling air cooling air cooling | 58~62 62~63 62~63 42~50 42~50 |
General quenching and tempering specifications: quenching temperature 1000~1050℃, quenching oil or quenching gas, hardness ≥ 60HRC; tempering temperature 160~180℃, tempering time 2h, or tempering temperature 325~375℃, tempering times 2 ~3 times.
1) Critical point temperature (approximate value): Ac1=730°C, Ac3=800°C, Ms=310°C.
2) Linear expansion coefficient: temperature 20~100°C/20~200°C/20~300°C/20~400°C/20~500°C/20~600°C,
Linear expansion coefficient: 11.1×10K/12.1×10K/12.9×10K/13.5×10K/13.9×10K14.1×10K.
3) Modulus of elasticity: temperature 20°C/300°C/400°C/500°C/600°C,
Elastic modulus 210000MPa/185000MPa/ 175000MPa/165000MPa/15500oMPa
Hot Working Specifications
The heating temperature is 1150 ~ 1200°C, the starting temperature is 1130 ~ 1180°C, the end temperature is > 850°C, and when φ> 50mm, slow cooling.
Normalizing Specification
The normalizing temperature is 850~900°C, and the oven is air-cooled.
High temperature tempering specification
The tempering temperature is 680~700°C, and the furnace is air-cooled.
Quenching and Tempering Specifications
Preheating temperature 680~700°C, quenching temperature 840~880°C, oil cooling, tempering temperature 580°C, water cooling or oil cooling, hardness ≤217HBW.
Specification for sub-temperature quenching and toughening treatment
Quenching temperature 900°C, tempering temperature 560°C, hardness (37±1) HRC
Induction hardening and tempering specification
The quenching temperature is 900°C, the tempering temperature is 150~180°C, and the hardness is 54~60HRC.
It is suitable for making large and medium-sized plastic molds that require certain strength and toughness.
Product display


keyword: | ASTM A106B A53 API 5L Seamless steel pipe |
Standard: | ASTM, DIN, GB, JIS |
Standard2: | ASTM A106-2006, ASTM A312M-2001, ASTM A312M-2007, ANSI A213M-2001, DIN 2391, DIN EN 10305, GB/T 3639-2000, GB/T 3093-2002, JIS G3460-2006, JIS G3467-2006 |
Grade Group: | 10#-45#, 16Mn, A53-A369, Cr-Mo alloy, Q195-Q345, ST35-ST52 |
Grade: | 10#, 20#, 45#, 16Mn, A53(A,B), A106(B,C), 30CrMo, Q345, St37, St45, ST37.4, ST54 |
Thickness: | 1 - 50 mm |
Section Shape: | Round |
Outer Diameter(Round): | 6 - 500mm |
Place of Origin: | China |
Application: | Hydraulic Pipe |
Technique: | Cold Rolled |
Surface Treatment: | anti-rust oil |
Special Pipe: | Thick Wall Pipe |
Secondary Or Not: | Non-secondary |
Material: | carbon/alloy/stainless steel |
Specification: | custom-made |
Delivery: | within 7--15 days |
Sample: | for free |
Port: | Shanghai Port,Tianjin Port,Ningbo Port |
Property: | well-controlled |
Length: | 5.8m-12m |
Ends: | Plastic cap |
FAQ
Q:What is your terms of payment?
A:We usually accept T/T in advance, L/C for large sum.If you prefer other payments terms, please discuss.
Q:What is the terms of delivery?
A:EXW, FOB, CIF
Q:What is the terms of packing?
A:Generally, we pack our goods in bundles or coils with rods or belts, we could also pack the goods as the customers' requirements.
Q:What is your delivery time?
A:For products in stock, we can ship it within 7 days after receiving the deposit.For custom order, production time is 15-30
workdays after received the deposit.
Q:Could you produce according to the samples?
A:Yes, we could customer-made by your samples or technique drawings, we could build the mold and fixtures.
Q:Can I place an sample order and what is your MOQ if I accept your quality?
A:Yes, we can send you samples but you may pay the express fees, our MOQ is 1 ton.
Q:How could you guarantee your products?
A:We accept and support the third-party inspection.We also could issue the warranty to customer to guarantee the quality.
Q:Where is the port of shipment?
A:Ningbo or Shanghai sea port.
Q:How can I get the price of needed product?
A:It's the best way if you can send us the material, size and surface, so we can produce for u to check the quality.If you
still have any confusion, just contact us, we would like to be helpful.